Trinic multi component powdered admixture pre-blended with Trinic white silica fume simplifies the production of GFRC, RPC, and ECC, no more mixing and matching several different admixtures at different dosage rates to produce high performance GFRC, RPC, and ECC.

Very easy to dose, less chance for human error

Eliminates the overnight shipping costs, foaming, and moldy product problems associated with liquids.

Contains a high-quality UV stable micro polymer specifically designed for GFRC production, eliminates the need for a 7-day wet cure (proven through independent testing).

Anti-foaming agents eliminate pinholes.

Improve color dispersion, intensity, and stability resulting in better color “pop”.

Contains specialized additives for water reduction.

Helps eliminate surface crazing, bowing, and curling.

Closes the internal capillaries within the GFRC matrix leading to a denser, more acid and stain resistant concrete.

Mixes faster than traditional GFRC, less cement clumps, more homogeneous mixes even with less than ideal mixers.

DOSAGE RECOMMENDATIONS:

Replace 10% to 15% of your cement with Trinic Pozz Plus

MIX DESIGN:

Face Coat:
  • 49.5# Portland Cement
  • 6.43#  Trinic GFRC Pozz Plus
  • 45# Sand
  • Water to Cement Ratio  – 0.30 to 0.34  ((total Cementitious in this example 49.5 + 6.43)
  • Trinic Stage II accelerator 1-4% of cementitious weight (optional if a faster strength gain is desired) dissolve into the mix water when dosing.
  • Fiber (optional) HD anti Crack 0.5% of the total dry weight of the mix.
Back Coat: 
  • 45# Portland Cement
  • 5.85#  Trinic GFRC Pozz Plus
  • 50# Sand
  • Water to Cement Ratio – 0.30 to 0.34 (total Cementitious in this example 45 + 5.85)
  • Trinic Stage II accelerator 1-4% of cementitious weight (optional if a faster strength gain is desired) dissolve into the mix water when dosing.
  • Fiber (Cem-Fil glass) 3% of total dry weight ingredients above.  OPTIONAL is use 0.5% HD fiber and 2% Cem-Fil glass fiber
Self-Consolidating:
  • Mix is the same as above with the addition of  Trinic Plasticizer at 0.25% to 0.75% of the total cementitious content.
Light Weight :
  • 45# white portland cement
  • 50# Q-Rok sand (weigh out the sand needed and replace some sand with the equal volume of Trinic light weight aggregate) Replace values can be up to 100% sand replacement depending on strength required)
  • 5.85#  Trinic GFRC Pozz Plus
  • Trinic Plasticiser 0.5% - 0.75% of cementitious weight (total Cementitious in this example 45 + 5.85)
  • Trinic Stage II accelerator 1-4% of cementitious weight (optional if a faster strength gain is desired) dissolve into the mix water when dosing.
  • Fiber 3% of total dry weight ingredients above
  • Water 30% of the cementitious weight (.3 water/ cement ratio)